HDPIR Polyisocyanurate Foam Material Pipe Shell For Nuclear Power
| Name: | HDPIR Pipe Shell For Nuclear Power |
|---|---|
| DENSITY: | 160-550 K |
| Thermal Conductivity (+20℃): | ≤0.035-≤0.085 W/(m·K) |
Customized Size High Density Polyisocyanurate Insulation Good Thermal Stability
| Application: | Liquefied Gas Plant |
|---|---|
| Name: | High Density Polyisocyanurate Insulation |
| Feature: | Customized |
Flame Resistant Polyisocyanurate Foam Pipe Insulation For Liquefied Gas Plant
| Name: | High Density Polyisocyanurate Insulation |
|---|---|
| Feature: | Low Water Absorption |
| Application: | Liquefied Gas Plant |
Durable High Density Polyisocyanurate Insulation Good Flammability Resistance
| Closed Cell Ratio: | ≥95% |
|---|---|
| Name: | Good Flammability Resistance |
| Feature: | Low Water Absorption |
High Strength Rigid Polyiso Foam Insulation Industrial Thermal Insulation Solution
| Operating Temperature Range: | -40°C To 120°C |
|---|---|
| Thermal Conductivity: | 0.02 W/mK |
| Material: | Polyisocyanurate Foam |
Low Linear Expansion Pipe Insulation Materials PIR Cryogenic Insulation 30 kg/m3
| Operating Temperature Range: | -40°C To 120°C |
|---|---|
| Thermal Conductivity: | 0.02 W/mK |
| Material: | Polyisocyanurate Foam |
Fireproof Polyisocyanurate Spray Foam Insulation Wide Operating Temperature Range
| Feature: | Fireproof |
|---|---|
| Application: | Liquefied Gas Plant |
| Name: | High Density Polyisocyanurate Insulation |
Fire Safety Pipe Insulation Materials PIR Insulation Board Customizable Thick
| Operating Temperature Range: | -40°C To 120°C |
|---|---|
| Thermal Conductivity: | 0.02 W/mK |
| Material: | Polyisocyanurate Foam |
Colorful Polyisocyanurate Rigid Foam Insulation For Liquefied Gas Plant
| Name: | Polyisocyanurate Rigid Foam Insulation |
|---|---|
| Feature: | Low Water Absorption |
| Application: | Liquefied Gas Plant |
Fireproof PIR Pipe Insulation Sections Polyisocyanurate Foam Sheets Tubular Shell Design
| Operating Temperature Range: | -40°C To 120°C |
|---|---|
| Thermal Conductivity: | 0.02 W/mK |
| Material: | Polyisocyanurate Foam |